code |
description |
mix ratio
[pbw]
|
cream time
[sec]
|
end expansion
[sec]
|
free rise density
[g/l]
|
tech data sheet
|
PU8228 |
HFO expanded foam for thermal insulation block. |
84:110 |
30 |
300 |
32 |
|
PU8229 |
PIR system for the production of thermal insulation blocks. |
89:210 |
35 |
150 |
27 |
|
PU8400 |
HFO expanded foam for discontinuos sandwich panels.
|
100:143 |
8 |
210 |
27 |
|
PU8401 |
Methyl formate expanded foam, designed for boilers.
|
100:130 |
20 |
180 |
32 |
|
PU8404 |
Water expanded foam, slow reactivity, ratio 1 to 1 in volume.
|
100:115 |
30 |
240 |
35 |
|
PU8405 |
HFO expanded foam for moulding. Compressive strength 127 kPa. |
100:100 |
20 |
60 |
50 |
|
PU8407 |
Methyl formate expanded foam, for moulding, ratio 1 to 1 in volume. |
100:120 |
25 |
210 |
45 |
|
PU8408 |
System expanding in contact with water. Ratio 1 to 1 in volume. Designed for waterproofing and consolidation of rocks and friable soils. |
100:117 |
12 |
52 |
35 |
|
PU8408FR |
Self-extinguishing version of PU8408. Ratio 1 to 1 in volume. Designed for waterproofing and consolidation of rocks and friable soils. |
100:115 |
10 |
70 |
70 |
|
PU8410 |
HFO expanded foam for moulding. Compressive strength 830 kPa. |
100:100 |
25 |
70 |
100 |
|
PU8411 |
HFO expanded foam, slow reactivity. Designed for fillings. |
100:100 |
60 |
480 |
52 |
|
PU8413 |
Water expanded foam, for moulding. Compressive strength 700 kPa. |
100:112 |
29 |
170 |
83 |
|